Coating

Coating Type Thickness SST Temp.&Humi PCT/HAST Use Temp
ZN 5-15 ≥48 / / ≤160ºC
NI 10-30 ≥96 ≥500 96 ≤200ºC
NI+Sn 10-30 ≥96 500 96 ≤200ºC
NI+Au 10-30 ≥96 500 96 ≤200ºC
NI+Ag 10-30 ≥96 72 48 ≤160ºC
Epoxy 10-30 ≥72 72 48 ≤160ºC
NICU+Epoxy 20-40 ≥500 500 200 ≤160ºC
NI+Epoxy 20-40 ≥500 500 200 ≤160ºC
Vaccum-plating AI 5-30 ≥100 500 200 ≤400ºC
AI+Epoxy 15-30 ≥200 500 200 ≤160ºC
Notes:corrosion resistance varies with the shape of the product

 

Due to the low corrosion resistance of NdFeB magnets, we need to do surface treatment before applications.

 The electroplating flows are as follow:

It may take a complete flow and a long time to do chamfering and cleaning, so electroplating needs a period to proceed.

The available coatings are as follows:
The most popular coatings are Zinc plating, Nickel plating, Epoxy and Passivation, the other coatings are Tin plating, Chromium plating, Gold plating, and Ag plating etc.